Features
Usage
Effects
# Features
· Strong penetration
· High gloss&hardness
· Small shrinkage after curing
· Wear-resistant&aging-resistant
· Weather resistance,acid&alkali resistance
· Environmentally friendly
# Usage
1.Stone repair areas should be clean, dry, and free of oil anddust.
2.A:B=2:1, the amount of glue added at one time should notexceed 10-20 grams.
3.The evenly mixed glue needs to be injected into the crackimmediately.
4.It takes 30 minutes for initial curing at room temperature of 25°C, and the next process can be started after 24 hoursIf possible, the glued plate should be heated to about 60°C for even heating. After being kept warm for 2-3 hours, it can be naturally cooled to room temperature before being polished.
Precaution
1.The construction temperature should be above 15℃ and the storage temperature should be above 0℃.
2.Avoid contact with eyes. If it accidentally enters eyes, please rinse with water immediately.
3.Do not take orally, please store in a cool, dry place out of reach of children.